ANSI\/ASME B36.10M, B36.19M Tykkelse Datatabel
May 12, 2025
Læg en besked
ANSI\/ASME B36.10M, B36.19M Tykkelse Datatabel
| Nominel størrelse (inches) | SCH5S | Sch10s | SCH10 | SCH20 | SCH30 | SCH40S | Std | SCH40 | SCH60 | SCH80S | Xs | SCH80 | SCH100 | SCH120 | SCH140 | SCH160 | Xxs | SCH160S |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 1/8 | 10.29 | - | 1.24 | - | - | 1.73 | 1.73 | 1.73 | 2.41 | 2.41 | 2.41 | - | - | - | - | - | - | - |
| 1/4 | 13.72 | - | 1.65 | - | - | 2.24 | 2.24 | 2.24 | 3.02 | 3.02 | 3.02 | - | - | - | - | - | - | - |
| 3/8 | 17.15 | - | 1.65 | - | - | 2.31 | 2.31 | 2.31 | 3.20 | 3.20 | 3.20 | - | - | - | - | - | - | - |
| 1/2(15) | 21.34 | 1.65 | 2.11 | - | - | 2.77 | 2.77 | 2.77 | 3.73 | 3.73 | 3.73 | - | - | - | 4.78 | 7.47 | 4.78 | - |
| 3/4(20) | 26.67 | 1.65 | 2.11 | - | - | 2.87 | 2.87 | 2.87 | 3.91 | 3.91 | 3.91 | - | - | - | 5.56 | 7.82 | 5.56 | - |
| 1(25) | 33.40 | 1.65 | 2.77 | - | - | 3.38 | 3.38 | 3.38 | 4.55 | 4.55 | 4.55 | - | - | - | 6.35 | 9.09 | 6.35 | - |
| 1 1/4(32) | 42.16 | 1.65 | 2.77 | - | - | 3.56 | 3.56 | 3.56 | 4.85 | 4.85 | 4.85 | - | - | - | - | 9.70 | - | - |
| 1 1/2(40) | 48.26 | 1.65 | 2.77 | - | - | 3.68 | 3.68 | 3.68 | 5.08 | 5.08 | 5.08 | - | - | - | - | 7.14 | 15.15 | 7.14 |
| 2(50) | 60.33 | 1.65 | 2.77 | - | - | 3.91 | 3.91 | 3.91 | 5.54 | 5.54 | 5.54 | - | - | - | - | 9.14 | 11.07 | 8.74 |
| 2 1/2(65) | 73.03 | 2.11 | 3.05 | - | - | 5.16 | 5.16 | 5.16 | 7.01 | 7.01 | 7.01 | - | - | - | - | 9.53 | 14.02 | 9.53 |
| 3(80) | 88.90 | 2.11 | 3.05 | - | - | 5.74 | 5.74 | 5.74 | 7.62 | 7.62 | 7.62 | - | - | - | - | 11.13 | 15.24 | 11.13 |
| 3 1/2(90) | 101.60 | 2.11 | 3.05 | - | - | 6.02 | 6.02 | 6.02 | 8.56 | 8.56 | 8.56 | - | - | - | 11.12 | 13.49 | 17.12 | 13.49 |
| 4(100) | 114.30 | 2.11 | 3.05 | - | - | 6.02 | 6.02 | 6.02 | 8.56 | 8.56 | 8.56 | - | - | - | 11.12 | 13.49 | 17.12 | 13.49 |
| 5(125) | 141.30 | 2.77 | 3.40 | - | - | 6.55 | 6.55 | 6.55 | 9.53 | 9.53 | 9.53 | - | - | - | 12.70 | 15.88 | 19.05 | 15.88 |
| 6(150) | 168.27 | 2.77 | 3.40 | - | - | 7.11 | 7.11 | 7.11 | 10.97 | 10.97 | 10.97 | - | - | - | 14.09 | 19.27 | 18.62 | 19.27 |
| 8(200) | 219.08 | 2.77 | 3.76 | 6.35 | 7.04 | 8.18 | 8.18 | 9.18 | 13.20 | 12.70 | 12.70 | 15.09 | 19.26 | 20.62 | 23.81 | 22.23 | 23.81 | |
| 10(250) | 273.05 | 3.40 | 4.19 | 6.35 | 7.80 | 9.27 | 9.27 | 9.27 | 12.70 | 12.70 | 12.70 | 15.09 | 19.26 | 21.44 | 25.40 | 28.58 | 25.40 | |
| 12(300) | 323.85 | 3.96 | 4.67 | 6.35 | 8.38 | 9.53 | 9.53 | 10.31 | 14.27 | 12.70 | 12.70 | 17.48 | 21.44 | 25.40 | 28.58 | 33.32 | 25.40 | |
| 14(350) | 355.60 | 3.96 | 4.78 | 6.35 | 7.92 | 9.53 | 9.53 | 11.13 | 15.09 | 12.70 | 12.70 | 19.05 | 23.81 | 27.79 | 31.75 | 35.71 | 25.40 | |
| 16(400) | 406.40 | 4.19 | 4.78 | 6.35 | 7.92 | 9.53 | 9.53 | 12.70 | 16.66 | 12.70 | 12.70 | 21.44 | 28.39 | 30.96 | 35.53 | 40.49 | 25.40 | |
| 18(450) | 457.20 | 4.19 | 4.78 | 6.35 | 7.92 | 11.13 | 9.53 | 14.27 | 19.05 | 12.70 | 12.70 | 23.81 | 29.36 | 34.33 | 38.67 | 45.24 | 25.40 | |
| 20(500) | 508.00 | 4.78 | 5.54 | 6.35 | 9.53 | 12.70 | 9.53 | 15.09 | 20.62 | 12.70 | 12.70 | 26.19 | 32.54 | 38.10 | 44.45 | 50.01 | 25.40 | |
| 22(550) | 558.80 | 4.78 | 5.54 | 6.35 | 9.53 | 12.70 | 9.53 | 22.23 | 12.70 | 12.70 | 28.58 | 34.93 | 41.26 | 47.63 | 53.98 | 25.40 | - | |
| 24(600) | 609.60 | 5.54 | 6.35 | 6.35 | 9.53 | 14.27 | 9.53 | 17.48 | 24.61 | 12.70 | 12.70 | 30.96 | 38.89 | 46.02 | 52.37 | 59.54 | - | |
| 26(650) | 660.40 | - | - | 7.92 | 12.70 | - | 9.53 | - | - | 12.70 | 12.70 | - | - | - | - | - | - | - |
| 28(700) | 711.20 | - | - | 7.92 | 12.70 | - | 9.53 | - | - | 12.70 | 12.70 | - | - | - | - | - | - | - |
| 30(750) | 762.00 | - | - | 7.92 | 12.70 | - | 9.53 | - | - | 12.70 | 12.70 | - | - | - | - | - | - | - |
| 32(800) | 812.80 | 6.35 | 7.92 | 7.92 | 12.70 | - | 9.53 | 17.48 | 12.70 | 12.70 | - | - | - | - | - | - | - | - |
| 34(850) | 863.60 | - | - | 7.92 | 12.70 | - | 9.53 | 17.48 | 12.70 | 12.70 | - | - | - | - | - | - | - | - |
| 36(900) | 914.40 | - | - | 7.92 | 12.70 | - | 9.53 | 19.05 | 12.70 | 12.70 | - | - | - | - | - | - | - | - |
| 40(1000) | 1016.00 | - | - | 9.53 | 14.3 | - | 9.53 | 26.20 | - | - | - | - | - | - | - | - | - | - |
Hvad er forskellen mellem nominelle og tommer rustfrie stålrør?
Nominel størrelse (DN):
Typisk udtrykt i millimeter (mm) henviser den nominelle størrelse til den omtrentlige diameter eller den indre diameter af røret.
Det er en nominel værdi, ikke den faktiske størrelse af røret. For eksempel,DN50angiver, at den nominelle diameter er cirka 50 mm, men den faktiske ydre diameter kan være60,3 mmafhængigt af vægtykkelsen.
Nominelle størrelser er vidt brugt i internationale standarder, især i Europa og Asien.
Tomme størrelse (NPS):
Udtrykt i tommer (tomme) henviser inch størrelsen til den nominelle rørstørrelse (NPS).
Denne navnekonvention bruges ofte i kejserlige systemlande som USA.
For eksempel,NPS 1Røret har en faktisk ydre diameter på33,4 mm, ikke 1 tommer (25,4 mm).
Send forespørgsel