EN10219-2/EN10296-2/EN10217-7 304 316 Stainless Steel Round Tube

Aug 04, 2025

Læg en besked

304 and 316 stainless steel tubesEN10219-2, EN10296-2, and EN10217-7 standards - ideal for architectural, industrial, structural, and fluid transportation applications

 

EN10219-2: Cold-formed welded structural hollow sections

EN10296-2

EN10217-7

and quality assurance documentation to meet international project specifications.

: 304 / 316
: EN10219-2 / EN10296-2 / EN10217-7

304 316 stainless steel pipe in stock

 

Spe.
304/316 EN10219-2 / EN10296-2 / EN10217-7 12 1.5 G600 / G320 / G240 / G180
304/316 EN10219-2 / EN10296-2 / EN10217-7 38.1 1.2 G600 / G320 / G240 / G180
304/316 EN10219-2 / EN10296-2 / EN10217-7 42.4 1.5 G600 / G320 / G240 / G180
304/316 EN10219-2 / EN10296-2 / EN10217-7 42.4 2.0 G600 / G320 / G240 / G180
304/316 EN10219-2 / EN10296-2 / EN10217-7 50.8 1.5 G600 / G320 / G240 / G180
304/316 EN10219-2 / EN10296-2 / EN10217-7 20×20 1.5 G600 / G320 / G240 / G180
304/316 EN10219-2 / EN10296-2 / EN10217-7 25×25 1.5 G600 / G320 / G240 / G180
304/316 EN10219-2 / EN10296-2 / EN10217-7 30×30 1.5 G600 / G320 / G240 / G180
304/316 EN10219-2 / EN10296-2 / EN10217-7 40×40 2.0 G600 / G320 / G240 / G180
304/316 EN10219-2 / EN10296-2 / EN10217-7 60×60 2.0 G600 / G320 / G240 / G180
304/316 EN10219-2 / EN10296-2 / EN10217-7 80×80 3.0 G600 / G320 / G240 / G180
304/316 EN10219-2 / EN10296-2 / EN10217-7 20×10 1.2 G600 / G320 / G240 / G180
304/316 EN10219-2 / EN10296-2 / EN10217-7 30×20 1.5 G600 / G320 / G240 / G180
304/316 EN10219-2 / EN10296-2 / EN10217-7 40×20 1.5 G600 / G320 / G240 / G180
304/316 EN10219-2 / EN10296-2 / EN10217-7 50×30 1.5 G600 / G320 / G240 / G180
304/316 EN10219-2 / EN10296-2 / EN10217-7 60×40 2.0 G600 / G320 / G240 / G180
304/316 EN10219-2 / EN10296-2 / EN10217-7 80×40 2.0 G600 / G320 / G240 / G180
304/316 EN10219-2 / EN10296-2 / EN10217-7 100×50 3.0 G600 / G320 / G240 / G180

EN10219-2/EN10296-2/EN10217-7 304 316 stainless steel round tube square tube rectangular tube